  I resprayed this 6M R.I.B with Aplha Plus in 2017.

  It was in a pretty bad state, the gelcoat had deep gouges on the bottom and there was quite a bit of filling to do. The deck had to be ground back to remove the Gelcoat printed grip.

  The entire boat was primed with Durepox white. The hull was painted in Awlcraft G-line Matterhorn white for a hard wearing, fast finish.

  The gunnels and consoles were also glossed in G-line Matterhorn white with Awlcraft G-line whisper grey non-skid.

​